Alexander Grabovetskiy, woodcarver, School of Woodcarving · Published 2020
What does a wood carver mean by "penetrates"?
Quick answer: In Venice Room workshop 77, part 9, I said the CA glue I used goes deep instead of sitting on top. In other lessons I said the word about diluted wood glue, a wood hardener, epoxy, primer, paint, stain, oil and light. For a glue I wanted on top, I said not penetrating.

In part 9 of workshop 77 of the Venice Room I said a thin CA glue is "not staying on the surface." My word for what it does was penetrates. I said it again in other lessons about wood glue thinned with water, a wood hardener, epoxy, primer, paint, stain and oil, and I said "not penetrating" about a glue I want to stay on top.
Do you carve thin petals that you hope will stay in one piece? Have you put stain over a spot where glue went in, and watched it blotch? Here are the places I said the word, and what came next.
What did the glue do in part 9?
The part opens on a leaf. "Maybe this one is a little too small," I said. "All right. Let me check the opposite side." And "here you go." The leaf "just curls up," I said, and it was not the final form: "we're still going to work on inside."
Next I told you about the glue: "super glue by this brand, it's probably the best I ever saw." After that, "It really stabilizes wood. It just actually gets inside of the fibers. It becomes a little solid." The brand was Starbond, I said: "It's a brand that's really thin, just like water."
On how it looks I said "You can see it, just liquidy on inside." And "Almost like water." Then came the word this page is named for: "And it's not staying on the surface, it actually penetrates right inside, and it's a really deep penetration." My next line was "So which makes it absolutely different from what I saw previously."
There was more to say. "I need to read a little more about this glue, by the way. Maybe it's not five years, maybe it's more." It was "a more professional-grade CA glue," I said, and "I was reading that even people who love to do marquetry, they're using it. It fills gaps between veneers. Feels really good."
Then my doubt: "I doubt those professional marqueters, people who's doing marquetry, they would use anything that is not going to last."
Why did I reach for the glue in part 8?
Part 8 of workshop 77 shows the reason. "And I almost broke it. Little too aggressive, I guess, today." Next: "Now, what I did, I actually fixed this part with the CA glue." The glue "stabilizes pretty much the wood and so on," and "that's a paint grade, so I really don't worry about it."
What I liked: "What I like about this glue, it penetrates all the way through." And "So it actually stabilizes this area, and that's really solid pretty much."
A limit came with it. "I have to find a solution how to reinforce the backside." On how long it lasts: "it's usually just about five years, 10 years at all. Depends on the brand." My plan had two halves: "I have to either glue that part to something else," or "reinforce it on the backside if I want to do the CA glue."
Part 10 shows the result. "And yes, I've got that CA glue inside, the fibers, and it's just really solid, almost like plastic. I didn't expect that." One side "slices really good with no problem." Near the break point, "it's actually like a plastic." Then a thought: "Maybe I should use that CA glue much more often and stabilize some of the work, or some of the areas, I should say."
Which small tool came next in part 9?
Back to the leaf. "And yes, I will make the divisions inside of each of those leaves. Again, I'm going to make three main divisions on inside of each of them." My reason: "Then it's going to look really interesting. Otherwise, it's just not too interesting at all."
For the relief cuts I had a plan: "So let me get relief cut right here. Relief cut, another relief cut, another relief cut, and I can get those separations done." About the tool: "It looks like I need to sharpen this tool." The area needs care. "I have to be super careful how I approach this area."
The tool itself was small. "I'm using a really small tool by Ashley Iles." It was "one of the detailing tools," and "There's multiple detailing tools, and you can probably catch on the background right here." The set is "not really micro tools, but those tools are made to work on details."
"I think it's excellent tools," I said, and "if you're really serious about creating some really unique stuff, I think it's something to consider to get those." On brand: "Not necessarily just that brand, but any other brand."
The handle? "this one has a really small handle, and it's really comfortable to hold." The tool "feels like almost pencil inside of your fingers, like you're holding a pencil or something."
A later step stayed a plan: "I'm going to take care of this with just a straight down cut and maybe with the smaller" tool, "maybe one-eighth of an inch or three millimeters."
Handles came up as well. About the micro tools I said "some of them really loose," and "some of them, you can actually pull out." My answer was CA glue, and "also epoxy can help you just hold it inside." The tools are still good, I said, "just the handles sometimes becoming loose."
Which thin glues did I say penetrate?
The word shows up in my other glue lessons. The short lesson on stabilizing a fragile part has it: "I used super glue. It's really thin, and it's by Starbond." Then "you penetrate that, and it actually goes all the way through all of those four ones." On raw wood: "if I would leave it just raw without any finish, I wouldn't use that glue."
The first Venetian flowers rosette lesson has the same glue on a knife edge. The edge is "a really fragile edge," I said, "like a knife edge." What to do: "all you do, you just pretty much just penetrate, and it just goes right inside." And "that stabilizes the edge."
My back cutting lesson gives three methods. "Before we flip that piece, we have to penetrate with something." Number one: "trusty Titebond wood glue." You "actually dilute that 50/50 with the water," and "It penetrates inside those resins." Then "it becomes more resin-like," I said, and that method is good "only if you're not planning to stain."
Number two is Starbond again. "And what you do, you just penetrate. It's really liquid-y." It "just penetrates, and it makes it stable." Of the method I said "Pretty much it's one of my favorite, favorite methods." For the paint, "great."
Does diluted wood glue penetrate too?
Roman acanthus lesson 11 is about going to the extreme, and I said "I usually don't use that technique, but you could." The technique: "You can dilute some glue, even yellow glue, just a carpenter's glue, like a Titebond," then "More water than glue, dilute it really good, and penetrate the fragile parts."
I added "You can penetrate with the glue the whole thing, actually." My reason: "Some resin gets inside," and "as those fibers are held together with those resins, with this glue, you can work more safely without it breaking." Even so, "You'll still be able to break it if you overdo it."
Workshop 95 of the Venice Room has me saying "I don't want to put any glue." Then "I mean, I could dilute some glue and penetrate that." The glue: "I kind of like lately talking about this Titebond glue. It is translucent glue." Its effect: "that's going to create a more rubbery, more solid." Then "You can stabilize the texture because there is a strong presence inside of that glue."
Which glue should stay on top of the wood?
Sometimes I do not want it to go in. Greek acroterion lesson 4 has a question about a paper pattern: "Some of you asking why I don't dilute my glue when I'm gluing my paper, when I'm gluing my design right on the top."
My answer: "When you dilute that glue with the water, it has a tendency to penetrate inside of the fibers of the wood." Under a stain finish I found out something: "even if you're sanding and you apply your stain, you can see some spots."
Glue from the bottle was another story. "I don't see that problem. You can see it's actually staying right on the top of my work piece, and it's not penetrating at all." "I found that's probably the best technique." For that job I'm using "just a regular Titebond," and "I wouldn't use Titebond 3."
Workshop 5 of the antique style rosette has a line about glue as well. Some glues are "really thin, and they are penetrating," and "I wouldn't use it if you are planning to finish it with some type of stain or lacquer because it's going to be noticeable." Normal yellow glue "will do the job," and it is "kind of thick, and that's not penetrating."
What did I say about epoxy and a wood hardener?
Tray of Blessing lesson 5 has an excavation underneath that "is already dangerous," and the reason, "the short grain and you can break it." On penetrating epoxy: "It's actually really good." You "could just brush and it just goes really deep." And "You don't have to penetrate the whole thing."
On a project of mine I said "that's fragile," and "you can easily break it." But "I actually brushed on the penetrating epoxy." What I said about the look: "the epoxy, it's a plastic look," and "that's why I don't like the epoxy itself."
Grape onlay lesson 10 has this line: "especially if you can penetrate that," then "penetrating epoxy on those fragile parts, they're gonna be stabilized and it's gonna stay forever, I guess, because it's a plastic and an epoxy."
The third method in the back cutting lesson: "In my case, I use a wood hardener." I added "I'm not sponsored by anyone." The hardener "penetrates really deeply on inside and dries really quickly." "I penetrate twice, sometimes three times. But after that stuff, you're still able to stain it, okay, and it's stable."
That lesson has a time limit too. "Super glue, the lifespan of the super glue, I think it's about five years. Maybe it's better now. I'm not sure." The Tray lesson names CA glue with "five years span."
Do paint, primer, stain and oil penetrate too?
They do, in my words. In Venice Room workshop 35 digging too deep would leave it really weak, I said, "which is okay also because later on it's still going to be painted." And "the paint itself going to penetrate and make it harder."
Floral and molding lesson 13 has a primer plan, and the project "will be painted, and that's not just penetrating paint." I planned "primer, maybe even two times," with "a really thick primer." My plan came with a reason: "really close to the level of shoulder. They could damage it."
And a wish: "I want to make sure that the primer penetrates completely," and "pretty much as much as possible." Tiny parts got a mention: "like the tiny petals," then "completely penetrated with the primer."
Workshop 112 brings up the grade of the wood. For a part that gets too fragile, "I can always reinforce it," with "glue diluted with water and penetrate it with the glue." Then "a paint grade, so it should not create any problem. If it would be a stain grade, then it would be blotchy."
Stain has its own lines. The kitchen cutting board, lesson 17, has it: "I'm going around and just checking if I left any white spots where my stain did not penetrate." Then "I'm not afraid to leave a little more on inside my stain," with "a little longer to dry it."
Oil comes in lesson 18 of the same board: "actually penetrate with that oil." Then "I have to feed it about three, four times until you're going to really see nice sheen on it." After that, "leave it for about a week until it dries before I can use it."
Wood bleach has the word in lily box lesson 13: "the first part, it penetrates deeply, same like water almost, and it's hard to hit the edges."
Can light, a tool or a marker penetrate?
Light does, in my words. In grape onlay lesson 5 I asked "Can you see that light penetrates right inside?" The Greek acanthus leaf, lesson 11, says "I just like when the light hits and you can see the light actually penetrates and goes through."
A tool can, too. Furniture panel lesson 19 has a finger on the molding: "it just gives me really, really good control," and it shows "how deeply my tool going to penetrate." That is "one of the ways to control it."
In furniture panel lesson 21 the markers go the other way: "they not penetrating." The same markers are "not permanent, and they're not really penetrating too deep."
The lines side by side
| Which lesson | What went into the wood | A line from the lesson |
|---|---|---|
| Venice 77 | Thin CA glue in a small carved leaf piece | "a really deep penetration" |
| Rosette 1 | Thin glue on a fragile knife edge | "goes right inside" |
| Back cutting | Titebond diluted with water, brushed on before flipping | "it becomes more resin-like" |
| Roman 11 | Carpenter's glue, diluted, for the fragile parts | "penetrate the fragile parts" |
| Acroterion 4 | A plain Titebond, under a paper pattern | "not penetrating at all" |
| Tray 5 | Penetrating epoxy, brushed on a fragile project | "goes really deep" |
| Back cutting | A wood hardener, applied twice or three times | "dries really quickly" |
| Venice 35 | Paint, as I expected it to go in | "penetrate and make it harder" |
| Floral 13 | A really thick primer, planned for tiny petals | "completely penetrated with the primer" |
| Kitchen 17 | A stain left a little heavier on the board | "a little longer to dry" |
| Greek 11 | Light, in a lesson on the Greek acanthus | "light actually penetrates and goes through" |
Wikipedia has pages on CA glue, epoxy and wood glue. Others cover wood stain, lacquer, shellac, wood finishing, paint and linseed oil. For this part's own words there is marquetry, veneers, gouges and pencil, and one gives the wide view of wood carving.
Where can you watch these lessons?
This part is in Venice Room 77, and Venice Room Part 7 holds workshops 74 to 85. The other glue lessons are the short one on stabilizing, back cutting and Roman acanthus 11. Planning a stain, a lacquer or paint? Look at what goes into the wood before you pick the glue.
How it's done
- Pick the glue by the finish. In my lesson on back cutting, Titebond and Starbond are for work with no stain planned, and a wood hardener let me stain after.
- Thin carpenter's glue for fragile parts. In Roman acanthus lesson 11 I said you can dilute the glue, even a yellow one, and use it on the fragile parts.
- Watch parts 8 and 10 for the glue. Part 8 of workshop 77 shows the glue going through the piece. Part 10 shows it slicing really good, then like plastic near the break point.
- Keep paper glue on top. Greek acroterion lesson 4 uses a regular Titebond, and it stayed on the work piece.
Frequently asked questions
Which glue did I name in part 9 of workshop 77?
Starbond, which is thin like water. It stabilizes wood, I said, and reaches into the fibers. Part 8 adds what I like about it: it penetrates through, and the area is really solid. Part 10 calls it almost like plastic.
Why not thin the glue for a paper pattern?
The Greek acroterion course, lesson 4, has me saying diluted glue tends to penetrate the wood, and under a stain finish I found you can see some spots. Glue straight out of the bottle stays on the work piece, I'm using a regular Titebond for the paper.
Can I stain over thin glue?
The Titebond and Starbond methods I showed for back cutting were good only if you're not planning to stain. For paint, great. When a stain is planned I use a wood hardener, and after that stuff I can still stain it.

About the author
Alexander Grabovetskiy
Master Wood Carver · Founder, School of Wood Carving
Alexander Grabovetskiy is a master wood carver, named International Woodcarver of the Year. He carves classical relief the old way, from acanthus leaves to full Baroque ornament. He started the School of Wood Carving, a nonprofit, to hand these skills to anyone ready to pick up a gouge.
What to carve next
- Venice Room 77
- Venice Room Part 7
- Stabilizing a fragile part
- Venetian flowers rosette 1
- A simple tip for back cutting
- Roman acanthus 11
- Venice Room 95
- Venice Room 112
- Greek acroterion 4
- Antique style rosette 5
- Tray of Blessing 5
- Grape onlay 10
- Venice Room 35
- Floral and molding 13
- Kitchen board 17
- Kitchen board 18
- Lily box 13